Professional RPET plastic siamna lama tawnhriat nei .
RPET sheet-a hman theih tur option zau tak .
Original siamtu man tlawm zawk
Item | hlutna | unit | norm . |
---|---|---|---|
mechanical 1000 a ni. | |||
Tensile chakna @ yield . | 59 | MPA 10 a ni. | ISO 527 a ni. |
Tensile chakna @ break . | No break a awm lo . | MPA 10 a ni. | ISO 527 a ni. |
Elongation @ break . | >200 a ni tawh. | % a ni. | ISO 527 a ni. |
Tensile modulus hmanga elasticity . | 2420 | MPA 10 a ni. | ISO 527 a ni. |
Flexural chakna . | 86 | MPA 10 a ni. | ISO 178 a ni. |
Charpy notched impact chakna . | (*) a ni. | KJ.M-2 a ni. | ISO 179 a ni. |
charpy a awm lo . | No break a awm lo . | KJ.M-2 a ni. | ISO 179 a ni. |
Rockwell Hardness M / R Scale 1000 a ni. | (*) / 111 a ni. | ||
Ball indentation a awm em? | 117 | MPA 10 a ni. | ISO 2039 a ni a. |
Optical . | |||
light transmission . | 89 | % a ni. | |
Refractive index 1000 a ni. | 1,576 an ni. | ||
thermal 1000 a ni. | |||
Max a ni. Service temperature 1000 a ni.2024 | 60 | °C a ni a. | |
Vicat Softening Point - 10N a ni. | 79 | °C a ni a. | ISO 306 a ni. |
Vicat Softening Point - 50N a ni. | 75 | °C a ni a. | ISO 306 a ni. |
HDT A @ 1.8 MPa | 69 | °C a ni a. | ISO 75-1,2 a ni. |
HDT B @ 0.45 MPA a ni. | 73 | °C a ni a. | ISO 75-1,2 a ni. |
Linear thermal expansion x10-5 a coefficient a ni. | <6 a ni. | x10-5 a ni. oc-1. |